Machining of Uranium and Uranium Alloys Available to Purchase
By
James A. Aris
James A. Aris
Rockwell International
Search for other works by this author on:
-
Published:1989
Page range:
874 - 878
Abstract
This article focuses on the basic metallurgy and machining parameters of classes of depleted and enriched uranium alloys. It provides information on the health precautions applicable to the machining of depleted uranium alloys. The article also discusses tool wear and the types of tools used in uranium alloy machining.
You do not currently have access to this chapter.
Citation
James A. Aris, Machining of Uranium and Uranium Alloys, Machining, Vol 16, ASM Handbook, By ASM Handbook Committee, ASM International, 1989, p 874–878, https://doi.org/10.31399/asm.hb.v16.a0002192
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Introduction to Machining Processes
Machining
Uranium and Uranium Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Corrosion of Uranium and Uranium Alloys
Corrosion: Materials
Heat Treating of Uranium and Uranium Alloys
Heat Treating of Nonferrous Alloys
Machining
Metals Fabrication Understanding the Basics
Very High Density Metals
Metals Handbook Desk Edition (2nd Edition)
Machining of Beryllium
Machining
Environmentally Assisted Cracking of Uranium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Glossary of Terms: Composites
Composites
Metallography and Microstructures of Uranium and Its Alloys
Metallography and Microstructures