Machining
Die Threading
-
Published:1989
Abstract
This article discusses the types and operations of the most common machines used for die threading. The construction, types, and comparison of solid and self-opening dies are discussed. The article explains the modification of chasers for threading Monel shaft. The principal factors that influence thread quality, production rate, and cost in die threading are composition and hardness of work metal; accuracy and finish; thread size; obstacles, such as shoulders or steps; speed; lead control; and cutting fluid. The article examines these factors and describes the tools and cutting fluids used for pipe threading along with the severity of stop...
Sign in
ASM members
Member Sign InDie Threading, Machining, Vol 16, ASM Handbook, By ASM Handbook Committee, ASM International, 1989, p 296–302, https://doi.org/10.31399/asm.hb.v16.a0002143
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.