Abstract
This article discusses the three characteristics that are important in evaluating and selecting metals for thread rolling, namely, rollability, flaking, and seaming. It reviews the capabilities and limitations of flat-die rolling, radial-infeed rolling, tangential rolling, through-feed rolling, planetary thread rolling, continuous rolling, and internal thread rolling, as well as the rolling machines and dies used. The article describes the factors affecting die life and provides information on radial die load, seam formation, surface finish, and thread dimensions that are affected by the form of the thread. It explains the reasons for using fluids in thread rolling. The article concludes...
Sign in
ASM members
Member Sign InThread Rolling, Machining, Vol 16, ASM Handbook, By ASM Handbook Committee, ASM International, 1989, p 280–295, https://doi.org/10.31399/asm.hb.v16.a0002142
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.