Machining
Abstract
This article discusses the functions of the major components of a waterjet machining system. These include hydraulic unit, intensifier, accumulator, filters, water transmission lines, on/off valve, waterjet nozzles, abrasive waterjet nozzle, waterjet catchers, and fluid additives. The article reviews several variables that influence the WJM process, such as pressure, flow and nozzle diameter, stand-off distance, traverse rate, and type and size of abrasive. Advantages and disadvantages of waterjet and abrasive waterjet cutting are also discussed. The article describes the applications of waterjet and abrasive waterjet machining.
Sign in
ASM members
Member Sign InC.E. Johnston, Waterjet/Abrasive Waterjet Machining, Machining, Vol 16, ASM Handbook, By ASM Handbook Committee, ASM International, 1989, p 520–527, https://doi.org/10.31399/asm.hb.v16.a0002158
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!