Shaping and Slotting
-
Published:1989
Abstract
Shaping and slotting are used to remove metal from surfaces through the use of a single-point tool supported by a ram that reciprocates the tool in a linear motion against the workpiece. This article discusses the process capabilities of shaping and slotting with respect to the size and configuration of the workpiece. Shaping and slotting machines develop cutting action from a straight-line reciprocating motion between the tool and the workpiece. The article describes the types of shapers such as horizontal shaper and vertical shaper. It briefly discusses the applications of high-speed steel tools and carbide tools for shaping. The...
Sign in
ASM members
Member Sign InShaping and Slotting, Machining, Vol 16, ASM Handbook, By ASM Handbook Committee, ASM International, 1989, p 187–193, https://doi.org/10.31399/asm.hb.v16.a0002133
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.