The constitutive relations for metalworking include elements of behavior at ambient temperature as well as high-temperature response. This article presents equations for strain hardening and strain-rate-sensitive flow, with alternate sections on empirically determined properties, followed by the models of constitutive behavior. It provides a discussion on creep mechanisms involving dislocation and diffusional flow, such as the Nabarro-Herring creep and the Coble creep. The equations for the several creep rates are also presented. Research on the mechanism of the superplastic flow in fine-grain metals has encompassed many ideas, such as the diffusional creep, dislocation creep with diffusional accommodation at grain boundaries, and concepts of grain-mantle deformation. The article concludes with information on the kinetics of superplastic deformation processes, including low stress behavior, concurrent grain growth, and high stress behavior.

You do not currently have access to this chapter.
Don't already have an account? Register

or Create an Account

Close Modal
Close Modal