Skip Nav Destination
ASM Handbook
Metalworking: Bulk FormingAvailable to Purchase
Edited by
ASM International
Volume
14A
ISBN electronic:
978-1-62708-185-6
Publication date:
2005
Book Chapter
Hot Working Simulation by Hot Torsion Testing[1] Available to Purchase
By
Joseph R. Pickens
Joseph R. Pickens
Concurrent Technologies Corporation
Search for other works by this author on:
-
Published:2005
Abstract
This article summarizes the types of hot working simulation tests such as hot tension, compression, and torsion testing used in the assessment of workability. It illustrates the use of hot torsion testing for the optimization of hot working processes. The article concludes with information on some hot torsion application examples.
You do not currently have access to this chapter.
Citation
Joseph R. Pickens, Hot Working Simulation by Hot Torsion Testing, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, https://doi.org/10.31399/asm.hb.v14a.a0009012
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Torsion Testing to Assess Bulk Workability
Metalworking: Bulk Forming
Hot-Tension Testing
Metalworking: Bulk Forming
Hot Tension and Compression Testing
Mechanical Testing and Evaluation
Mechanical Behavior
Fatigue and Fracture Understanding the Basics
Useful Formulas for Deformation Analysis and Workability Testing
Metalworking: Sheet Forming
Stress Relaxation Testing
Mechanical Testing and Evaluation
Mechanical Testing
Metals Handbook Desk Edition (2nd Edition)
Recovery Hopkinson Bar Techniques
Mechanical Testing and Evaluation
Useful Formulas for Metals Processing
Metals Process Simulation
Mechanical Behavior
Elements of Metallurgy and Engineering Alloys