Forging Design Involving Ribs and Bosses
-
Published:2005
Publication history
April 04, 2006
Abstract
Ribs and bosses are the integral functional elements or features of a forging that project outward from a web in a direction parallel to the ram stroke. This article describes the design, functions, and producibility of ribs and bosses. It relates their design to grain flow, metallurgical structure, measurement details, and design parameters, with supplementary data obtained from the examples of actual forgings.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Forging Design Involving Ribs and Bosses, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 741–758, https://doi.org/10.31399/asm.hb.v14a.a0004038
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Forging Design Involving Parting Line and Grain Flow
Metalworking: Bulk Forming
Forging Design Involving Flash and Trim
Metalworking: Bulk Forming
Forging Design Involving Webs
Metalworking: Bulk Forming
Forging of Titanium Alloys
Metalworking: Bulk Forming
Forging Design Dimensions and Tolerances
Metalworking: Bulk Forming
Principles of Forging Machines
Cold and Hot Forging Fundamentals and Applications
Failures Related to Metalworking
Failure Analysis and Prevention
Temperature and Heat Transfer
Cold and Hot Forging Fundamentals and Applications
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Failure of Steel Missile Launcher Attachment Bolts
ASM Failure Analysis Case Histories: Air and Spacecraft