This article contains nine tables that present useful formulas for deformation analysis and workability testing. The tables present formulas for effective stress, strain, and strain rate in arbitrary coordinates, principal, compression and tension testing of isotropic material. The article also provides formulas for flat rolling, conical-die extrusion, wire drawing, deep drawing of cups from sheet metal, and bending, and formulas for anisotropic sheet materials.
Useful Formulas for Deformation Analysis and Workability Testing, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 827–830, https://doi.org/10.31399/asm.hb.v14a.a0004030