Nonferrous Hardness Conversions
-
Published:2005
Page range:
858 - 860
Abstract
This article presents a comprehensive collection of tables that list Rockwell hardness and superficial hardness numbers for wrought aluminum products, wrought coppers, and cartridge brass.
You do not currently have access to this chapter.
Citation
Nonferrous Hardness Conversions, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 858–860, https://doi.org/10.31399/asm.hb.v14a.a0004044
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Nonferrous Hardness Conversions
Metalworking: Sheet Forming
Steel Hardness Conversions
Metalworking: Bulk Forming
Steel Hardness Conversions
Heat Treating of Irons and Steels
Surface Engineering to Change the Surface Metallurgy
Surface Engineering for Corrosion and Wear Resistance
Alloy and Temper Designation Systems for Aluminum and Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Wrought Aluminum Alloys
Metals Handbook Desk Edition (2nd Edition)
Properties of Wrought Aluminum and Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Fractography of Aluminum Alloys
Fractography
Approximate Equivalent Hardness Numbers and Tensile Strengths for Rockwell C and B Hardness Numbers for Steel
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Hardness Conversions for Steels
Mechanical Testing and Evaluation