This article reviews the methods of machining and finishing forging dies. It illustrates different stages in die manufacturing. The article provides a brief description on requirements and characteristics of high-speed machining tools, including feed rates, spindle speed, surface cutting speeds, and high acceleration and deceleration capabilities. It discusses electrodischarge machining process and electrochemical machining process. The article concludes with information on die-making methods.