Metalworking: Bulk Forming
Design for Deformation Processing
-
Published:2005
Abstract
This article reviews the general aspects of product design and provides an overview of the manufacturing processes and their relationship to design, with an emphasis on deformation processes. It discusses the various classes of deformation processes to illustrate their impacts on product design while taking advantage of the benefits of deformation processing.
Sign in
ASM members
Member Sign InHoward Kuhn, Design for Deformation Processing, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 11–20, https://doi.org/10.31399/asm.hb.v14a.a0003972