Metalworking: Bulk Forming
Coextrusion
-
Published:2005
Abstract
Coextrusion is defined as the simultaneous extrusion of two or more metals to form an integral product that can be carried out using conventional extrusion or drawing equipment at a temperature appropriate to the metal system being formed. This article discusses the applications, billet configurations, and metal flow modes of coextrusion. It presents the analytical studies of coextrusion: deformation energy methods, lower-bound (slab) analyses, upper-bound analyses, and finite-element analyses. These studies are used to identify the regime of material properties and process variables for which sound extrusions can be obtained. The article concludes with a discussion on the state-of-the-art of coextrusion that assists in developing process models, which accurately describe both the macroscopic and microscopic aspects of a process.
Raghavan Srinivasan, Craig S. Hartley, Coextrusion, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 505–515, https://doi.org/10.31399/asm.hb.v14a.a0004013
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.