Failure Analysis and Prevention
The Failure Analysis Process: An Overview
-
Published:2002
Abstract
Failure analysis is a process that is performed to determine the causes or factors that have led to an undesired loss of functionality. This article describes some of the factors and conditions that might be considered when approaching a failure analysis problem. It focuses on the key principles, objectives, practices, and procedures of failure analysis. The article provides guidelines on the preparation of a protocol for a failure analysis. It also demonstrates the proper approaches to failure analysis.
Sign in
ASM members
Member Sign InDebbie Aliya, The Failure Analysis Process: An Overview, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 315–323, https://doi.org/10.31399/asm.hb.v11.a0003518
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!