Failure Analysis and Prevention
Fracture Modes and Appearances in Ceramics
-
Published:2002
Abstract
Fractography is the means and methods for characterizing a fractured specimen or component. This includes the examination of fracture-exposed surfaces and the interpretation of the fracture markings as well as the examination and interpretation of crack patterns. This article describes the former of these two parts of fractography. It presents the techniques of fractography and explains fracture markings using glass and ceramic examples. The article also discusses the fracture modes in ceramics and provides examples of fracture origins.
Sign in
ASM members
Member Sign InJames R. Varner, Fracture Modes and Appearances in Ceramics, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 662–670, https://doi.org/10.31399/asm.hb.v11.a0003542
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!