Abstract
This article describes the two critical goals in a failure investigation: damage mechanisms and damage modes. It explains the determination of primary and secondary damage mechanisms and discusses the methodology used to classify the damage mechanisms.
You do not currently have access to this chapter.
Citation
Aaron Tanzer, Determination and Classification of Damage, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 343–350, https://doi.org/10.31399/asm.hb.v11.a0003521
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Determination and Classification of Damage
Failure Analysis and Prevention (2021 Edition)
What Is a Failure?
How to Organize and Run a Failure Investigation
Organization of a Failure Investigation
Failure Analysis and Prevention
Nine Steps of a Failure Investigation
How to Organize and Run a Failure Investigation
How to Organize and Run a Failure Investigation
Failure Analysis and Prevention (2021 Edition)
Data Review, Conclusions, and Report Preparation
Failure Analysis and Prevention (2021 Edition)
A Few Pitfalls and More Useful Tools
How to Organize and Run a Failure Investigation
Examination of Damage and Material Evaluation
Failure Analysis and Prevention (2021 Edition)
Aspects of a Failure Investigation
How to Organize and Run a Failure Investigation