Failures of Bridge Components[1]
By
John W. Fisher
John W. Fisher
Fritz Engineering Laboratory, Lehigh University
Search for other works by this author on:
-
Published:2002
Abstract
This article illustrates the defects, which result because of poor-quality welds in the bridge components. The cracks resulting from the use of low fatigue strength details are also discussed. The article describes the effect of out-of-plane distortion in floor-beam-girder connection plates, multiple-girder diaphragm connection plate, and tied-arch floor beams.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
John W. Fisher, Failures of Bridge Components, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, https://doi.org/10.31399/asm.hb.v11.a0001821
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Fatigue-Life Assessment
Analysis and Prevention of Component and Equipment Failures
Characterization of Welds
Weld Integrity and Performance
Analysis of Distortion and Deformation
Failure Analysis and Prevention (2021 Edition)
Residual Stresses, Distortion, and Heat Treatment
Steels: Processing, Structure, and Performance (Second Edition)
Distortion
Practical Nitriding and Ferritic Nitrocarburizing
Nondestructive Inspection of Tubular Products
Nondestructive Evaluation of Materials
Quality Control of Electron Beams and Welds
Welding Fundamentals and Processes
Press Quenching
Steel Heat Treating Fundamentals and Processes
Distortion Failures
Understanding How Components Fail (Third Edition)