Abstract
This article describes the failure characteristics of high-pressure long-distance pipelines. It discusses the causes of pipeline failures and the procedures used to investigate them. The use of fracture mechanics in failure investigations and in developing remedial measures is also reviewed.
You do not currently have access to this chapter.
Citation
R.J. Eiber, J.F. Kiefner, Failures of Pipelines, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, https://doi.org/10.31399/asm.hb.v11.a0001820
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Failure of a Buried Type 304L Stainless Steel Drain Line by Galvanic Attack
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Porous Coatings on Metallic Implant Materials
Materials for Medical Devices
Close-Interval Survey Techniques
Corrosion: Environments and Industries
Guided Wave Testing
Nondestructive Evaluation of Materials
Cracking of a Field Girth Weld
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Examination of a Blistered and Cracked Natural Gas Line
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Fracture Mechanics Testing of Plastics
Characterization and Failure Analysis of Plastics
Thermomechanical Fatigue: Mechanisms and Practical Life Analysis
Failure Analysis and Prevention
Concepts of Fracture Control and Damage Tolerance Analysis
Fatigue and Fracture
Modeling Fatigue Crack Growth
Fundamentals of Modeling for Metals Processing