Failures of Pipelines[1]
By
J.F. Kiefner
Battelle Columbus Laboratories
J.F. Kiefner
Search for other works by this author on:
-
Published:2002
Abstract
This article describes the failure characteristics of high-pressure long-distance pipelines. It discusses the causes of pipeline failures and the procedures used to investigate them. The use of fracture mechanics in failure investigations and in developing remedial measures is also reviewed.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
R.J. Eiber, J.F. Kiefner, Failures of Pipelines, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, https://doi.org/10.31399/asm.hb.v11.a0001820
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Failure of a Buried Type 304L Stainless Steel Drain Line by Galvanic Attack
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Porous Coatings on Metallic Implant Materials
Materials for Medical Devices
Cracking of a Field Girth Weld
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Examination of a Blistered and Cracked Natural Gas Line
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Close-Interval Survey Techniques
Corrosion: Environments and Industries
Guided Wave Testing
Nondestructive Evaluation of Materials
Thermomechanical Fatigue: Mechanisms and Practical Life Analysis
Failure Analysis and Prevention
A Fracture Mechanics Based Failure Analysis of a Cold Service Pressure Vessel
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Application of Fracture Mechanics to Pipeline Failure Analysis
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Concepts of Fracture Control and Damage Tolerance Analysis
Fatigue and Fracture