Abstract
This article discusses the effect of using unsuitable alloys, metallurgical discontinuities, fabrication practices, and stress raisers on the failure of a pressure vessel. It provides information on pressure vessels made of composite materials and their welding practices. The article explains the failure of pressure vessels with emphasis on stress-corrosion cracking, hydrogen embrittlement, brittle and ductile fractures, creep and stress rupture, and fatigue with examples.
Topics
Corrosion,
Material failure analysis,
Wear,
Formability testing,
Life assessment testing,
Root cause analysis,
Brittle fracture,
Stress corrosion cracking,
Creep fracture,
Ductile fracture,
Hydrogen embrittlement,
Manufacturing defects,
Pressure vessels,
Composites,
Stress rupture testing,
Welding,
Fatigue properties,
Failure mechanisms and analysis,
Processing, treatment, and fabrication
You do not currently have access to this chapter.
Citation
Roy T. King, Failures of Pressure Vessels, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, https://doi.org/10.31399/asm.hb.v11.a0001818
Download citation file:
Related Book Content
Fracture Mechanics and Service Fitness of Welds
Weld Integrity and Performance
Fitness-for-Service Assessment of Welded Structures
Welding, Brazing, and Soldering
Stress-Corrosion Cracking of Stainless Steels
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Failure Analysis of Steel Welds
Failure Analysis of Heat Treated Steel Components
Corrosion of Ferritic Stainless Steel Weldments
Corrosion of Weldments
Stress-Corrosion Cracking of Amorphous Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Ductile and Brittle Fracture
Fatigue and Fracture Understanding the Basics
Deformation and Fracture Mechanisms and Static Strength of Metals
Mechanics and Mechanisms of Fracture An Introduction
Fracture and Fractography
Characterization and Failure Analysis of Plastics
Failures of Gears
Failure Analysis and Prevention