Materials Selection for Failure Prevention Available to Purchase
-
Published:2002
Abstract
Materials selection is an important engineering function in both the design and failure analysis of components. This article briefly reviews the general aspects of materials selection as a concern in proactive failure prevention during design and as a possible root cause of failed parts. It discusses the overall concept of design and describes the role of the materials engineer in the design and materials selection process. The article highlights the significance of materials selection in both the prevention and analysis of failures.
Brett A. Miller, Materials Selection for Failure Prevention, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 24–39, https://doi.org/10.31399/asm.hb.v11.a0003501
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.