Fundamentals of Wear Failures
By
Raymond G. Bayer
Raymond G. Bayer
Tribology Consultant
Search for other works by this author on:
-
Published:2002
Publication history
November 01, 2002
Abstract
This article focuses on the types of activities required for the resolution of wear problems. These include examining and characterizing the tribosystem; characterizing and modeling the wear process; obtaining and evaluating wear data; and evaluating and verifying the solution.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Raymond G. Bayer, Fundamentals of Wear Failures, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 901–905, https://doi.org/10.31399/asm.hb.v11.a0003558
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Impact Wear Failures
Failure Analysis and Prevention (2021 Edition)
Failures from Various Mechanisms and Related Environmental Factors
Metals Handbook Desk Edition (2nd Edition)