Abstract
This article is a compilation of tables that provide information on preheat and interpass temperatures and the postweld heat treatment for selected carbon steels, as well as steel pressure vessels and pipe welds. Information is also provided for preheat and interpass temperatures of heat treatable steels, namely, low-alloy steels and ultra high-strength steels.
You do not currently have access to this chapter.
Citation
Preheat and Postweld Heat Treatment Temperatures for Selected Steels, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 878–881, https://doi.org/10.31399/asm.hb.v06a.a0005645
Download citation file:
Related Book Content
Influence of Welding on Steel Weldment Properties
Welding, Brazing, and Soldering
Corrosion of Cast Carbon and Low-Alloy Steels
Corrosion: Materials
Brittle Fracture Assessment and Failure Assessment Diagrams
Analysis and Prevention of Component and Equipment Failures
Stress-Corrosion Cracking of Weldments in Boiling Water Reactor Service
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Reference Tables
Weld Integrity and Performance
Introduction to the Selection of Carbon and Low-Alloy Steels
Welding, Brazing, and Soldering
Fatigue and Fracture Resistance of Heat-Resistant (Cr-Mo) Ferritic Steels
Fatigue and Fracture
Postweld Heat Treatment of Nonferrous High-Temperature Materials
Welding, Brazing, and Soldering
Selection of Nickel-Base Corrosion-Resistant Alloys Containing Molybdenum
Welding, Brazing, and Soldering