Submerged Arc Welding Available to Purchase
-
Published:2011
Abstract
Submerged arc welding (SAW) is suited for applications involving long, continuous welds. This article describes the operating principle, application, advantages, limitations, power source, equipment, and fluxes in SAW. It reviews three different types of electrodes manufactured for SAW: solid, cored, and strip. The article highlights the factors to be considered for controlling the welding process, including fit-up of work, travel speed, and flux depth. It also evaluates the defects that occur in SAW: lack of fusion, slag entrapment, solidification cracking, and hydrogen cracking. Finally, the article provides information on the safety measures to be followed in this process.
Lee E. Allgood, Submerged Arc Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 335–343, https://doi.org/10.31399/asm.hb.v06a.a0005566
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.