Evaluation and Quality Control of Resistance-Welded Joints
-
Published:2011
Abstract
This article presents the structural attributes and internal characteristics of spot welds as well as the commonly inspected imperfections in resistance welds. It describes the industrial requirements for weld quality. Commonly performed destructive evaluations, namely, manual testing, quasi-static mechanical tests, dynamic mechanical tests, and metallographic examination, are reviewed. The article reviews weld-quality monitoring using various process signals and provides a discussion on the on-line and off-line nondestructive evaluation methods of spot weld quality.
Hongyan Zhang, Evaluation and Quality Control of Resistance-Welded Joints, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 486–503, https://doi.org/10.31399/asm.hb.v06a.a0005628
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.