Power Sources for Arc Welding
-
Published:2011
Abstract
This article describes the characteristics and technology of power sources for major arc welding methods along with the suggested criteria for assuring that a power source selection can safely deliver the desired output and yield long service life. Power sources with single-phase AC input voltage, three-phase input machines, inverter-based power sources, short arc gas metal arc welding power sources, and multiple arc power sources are discussed. The article also presents the factors to be considered when selecting a power source.
Lee Allgood, Power Sources for Arc Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 277–284, https://doi.org/10.31399/asm.hb.v06a.a0005565