Heat Flow in Fusion Welding[1]
-
Published:2011
Abstract
The finished product, after fusion welding, may contain physical discontinuities due to excessively rapid solidification, adverse microstructures due to inappropriate cooling, or residual stress and distortion due to the existence of incompatible plastic strains. To analyze these problems, this article presents an analysis of the welding heat flow, with focus on the fusion welding process. It discusses the analytical heat-flow solutions and their practical applications. The article concludes with a description of the effects of material property and welding condition on the temperature distribution of weldments.
Chon L. Tsai, Heat Flow in Fusion Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 55–66, https://doi.org/10.31399/asm.hb.v06a.a0005588
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.