This article provides information on the practice considerations for the inertia and direct-drive rotary friction welding processes. It presents the tooling and welding parameter designs of these processes. The article discusses the welding of different material family classes to provide a baseline for initial development of a welding parameter set. Common material family classes, including steels, nonferrous metals, and dissimilar metals, are discussed.

This article lists the system parameters of the friction welding process and describes the four categories of monitoring and control of the manufacturing process. It discusses the monitoring methods of a rotary friction welded sample,...