Welding Fundamentals and Processes
High Energy Electron Beam and Laser Beam Welding
-
Published:2011
Abstract
This article provides a history of electron and laser beam welding, discusses the properties of electrons and photons used for welding, and contrasts electron and laser beam welding. It presents a comparison of the electron and laser beam welding processes. The article also illustrates constant power density boundaries, showing the relationship between the focused beam diameter and the absorbed beam power for approximate regions of keyhole-mode welding, conduction-mode welding, cutting, and drilling.
Abstract
This article introduces the operating principles and modes of operation for high-vacuum (EBW-HV), Medium-vacuum (EBW-MV), and nonvacuum (EBW-NV) electron beam welding. Equipment, process sequence, part preparation,...
Sign in
ASM members
Member Sign InHigh Energy Electron Beam and Laser Beam Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011
Download citation file: