Welding Fundamentals and Processes
Fundamentals of Welding
-
Published:2011
Abstract
Joining is key to the manufacture of large or complex devices or assemblies; construction of large and complex structures; and repair of parts, assemblies, or structures in service. This article describes the three forces for joining: physical, chemical, and mechanical. It provides an overview of the joining processes, namely, mechanical fastening, integral attachment, adhesive bonding, welding, brazing, and soldering. The article concludes with information on the various aspects of joint design and location that determine the selection of a suitable joining method.
Abstract
This article overviews the classification of welding processes and the key process embodiments for joining by...
Sign in
ASM members
Member Sign InFundamentals of Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.