In most castings, there are junctions between intersecting component members. This article describes how defects can be eliminated in five types of junctions in steel castings, namely the L-junction, T-junction, V-junction, X-junction, and Y-junction. It also discusses design considerations for junctions in aluminum castings and provides a comparison between the T-junction and Y-junction. Finally, the article illustrates recommended methods for minimizing defects where sections of unequal thickness form a junction.