Transfer and Treatment of Molten Metal—An Introduction Available to Purchase
-
Published:2008
Abstract
This article discusses various molten-metal treatments, namely fluxing, degassing, and molten-metal filtration. It focuses on various molten-metal handling systems for transporting, holding, or delivering molten metal to the mold/die system. These include launders, tundishes, holding furnaces or transport crucibles, molten-metal transfer pumps, teeming ladles, and dosing and pouring furnaces.
Transfer and Treatment of Molten Metal—An Introduction, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 173–184, https://doi.org/10.31399/asm.hb.v15.a0005352