Steel Castings Properties Available to Purchase
Revising author
-
Published:2008
Abstract
This article discusses the mechanical properties of carbon steels, low-alloy steels, wear-resistant steels, corrosion-resistant steels, heat-resistant steels, and common alloys at both room and elevated temperature. It also provides information on the corrosion-resistant and heat-resistant applications of the common alloys.
David Poweleit, Steel Castings Properties, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 949–974, https://doi.org/10.31399/asm.hb.v15.a0005329
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.