Abstract
This article discusses the types of patterns used for a specific application such as loose patterns, match plate patterns, cope and drag patterns, and special patterns. It describes the principles of the patternmaking techniques used to make expendable molds and for metal casting processes such as die casting and permanent mold casting. The article reviews the pattern features and mold production considerations used in the pattern design, namely, parting line considerations, addition of gates and risers, core prints, and locating points. It examines the pattern allowances for ensuring a dimensionally correct final pattern. A variety of materials and advanced composite materials used in the manufacture of patterns are discussed. The article evaluates the factors influencing the selection of type of patterns for specific castings.
Robert C. Voigt, Patterns and Patternmaking, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 488–496, https://doi.org/10.31399/asm.hb.v15.a0005308
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.