Crucible Furnaces Available to Purchase
-
Published:2008
Abstract
This article discusses the design parameters, operation, characteristics, properties, and advantages of various types of crucible furnaces, such as stationary, tilting, and movable furnaces. It also provides information on the application of the crucible furnaces.
George Giles, Crucible Furnaces, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 155–159, https://doi.org/10.31399/asm.hb.v15.a0005198