Nonferrous Casting—An Introduction
-
Published:2008
Abstract
This article reviews the melt processing and casting of non-ferrous alloys, such as nickel alloys, titanium alloys, and lead alloys. It describes the lead refining steps, namely, copper drossing, softening, desilvering, zinc removal, bismuth removal, and final refining.
Nonferrous Casting—An Introduction, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 989–991, https://doi.org/10.31399/asm.hb.v15.a0005306