This article describes the principles and classifications of induction furnaces. The classifications of induction furnaces are coreless and channel. The electromagnetic stirring action in these furnaces is reviewed. The article provides information on the various power supplies and water cooling systems for induction furnaces. Furnace operators can increase the power supply utilization by the use of mechanical skimmers. The article describes the various lining materials used in induction furnaces, namely, silica, alumina, and magnesia. The crucible wall scrapers, ramming mixes, and lining push-out device used in induction furnaces are also reviewed. The article concludes with a discussion on batch...