High-Alloy Graphitic Irons
-
Published:2008
Abstract
This article discusses the melting and pouring practices, heat treatment, and applications of different types of high-alloy graphitic iron, namely, high-silicon gray irons, high-silicon ductile irons, nickel-alloyed austenitic irons, austenitic gray irons, austenitic ductile irons, and aluminum-alloyed irons.
Sign in
ASM members
Member Sign InRichard B. Gundlach, High-Alloy Graphitic Irons, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 904–908, https://doi.org/10.31399/asm.hb.v15.a0005328