Permanent Mold Casting
Revising author
Revising author
-
Published:2008
Abstract
This article provides information on metals that can be cast in permanent molds. It describes the advantages, disadvantages, applications, and design of permanent castings. Following a discussion on the factors considered in mold design and material selection, the article details the application of mold coatings and examines the effects of major processing variables on mold life. The variables that determine mold temperature and measures for controlling it are reviewed, and the effects of short-term and long-term variables on the dimensional accuracy of permanent mold castings are explained. The article concludes with a discussion on the factors influencing the surface finish on permanent mold castings.
Don Tyler, Robert Pischel, Permanent Mold Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 689–699, https://doi.org/10.31399/asm.hb.v15.a0005260
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.