Casting Failure Analysis Techniques and Case Studies Available to Purchase
-
Published:2008
Abstract
This article reviews the failure analysis process with specific reference to the considerations that should be addressed when a casting has failed. It describes the failure analysis methodology for three failed cast components: an aluminum bracket, a bronze suction roll, and a steel automotive spindle. The article discusses failure analysis investigation by obtaining casting background information, planning the evaluation and selecting the appropriate casting for analysis, conducting a preliminary examination, conducting the proper material evaluations, and thoroughly evaluating the test data. It concludes with information on case studies that show how the methodology is adapted for differing materials, failure mechanisms, and failure circumstances.
Craig Brown, Casting Failure Analysis Techniques and Case Studies, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 1183–1191, https://doi.org/10.31399/asm.hb.v15.a0005343
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.