Abstract
Nonplanar microstructures form most frequently during the solidification of alloys, and play a crucial role in governing the properties of the solidified material. This article emphasizes the basic ideas, characteristic lengths, and the processing conditions required to control the columnar and equiaxed microstructures. The formation of cellular and dendritic structures in one- and two-phase structures is presented with emphasis on the effect of processing conditions and composition on the selection of microstructure and microstructure scales.
Rohit Trivedi, Erin Sunseri, Non-Plane Front Solidification, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 299–306, https://doi.org/10.31399/asm.hb.v15.a0005210
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.