This article reviews the basic types of mold aggregates and bonding methods for expendable molds and coremaking. It provides an overview of mold media and the basic types of sands and their properties. The most significant clays used in green sand operations, such as bentonites, are discussed. The article describes the methods of sand bonding with inorganic compounds. It provides a description of resin-bonded sand systems: no-bake binder systems, heat-cured binder systems, and cold box binder systems. The article concludes with a discussion on the media used for expendable molds, namely, ceramic shells and rammed graphite, for casting reactive metals such as titanium or zirconium.
John Jorstad, Mary Beth Krusiak, John O. Serra, Vic La Fay, Aggregates and Binders for Expendable Molds, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 528–548, https://doi.org/10.31399/asm.hb.v15.a0005242
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.