Compacted Graphite Iron Castings Available to Purchase
-
Published:2008
Abstract
This article reviews the graphite morphology, chemical composition requirements, castability, mechanical properties, and corrosion resistance of compacted graphite (CG) irons. It describes the factors affecting the mechanical properties of CG irons. The article also presents the advantages of CG irons.
Compacted Graphite Iron Castings, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 872–883, https://doi.org/10.31399/asm.hb.v15.a0005325