Abstract
The commonly used nondestructive testing of cast products include liquid penetrant inspection, radiographic inspection, fluoroscopic inspection and automated defect recognition, ultrasonic inspection, eddy current inspection, process-controlled resonant testing (PCRT), leak test, and electrical conductivity measurements. This article summarizes the application of these nondestructive tests to castings. It also tabulates a partial list of automotive part types and materials amenable to PCRT and lists the potential limitations to the use of PCRT.
Rathindra DasGupta, Nondestructive Testing of Components, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 1174–1177, https://doi.org/10.31399/asm.hb.v15.a0005341
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.