This article discusses selected highlights of thermodynamic relationships during solidification and nucleation kinetics behavior in connection with the basis of nucleation treatments, such as grain refinement and inoculation, to provide a summary of nucleation phenomena during casting. The article describes nucleation phenomenon such as homogeneous nucleation and heterogeneous nucleation. It examines various grain refinement models, such as the carbide-boride model, the free growth model, and the constitutional undercooling model. The article concludes with information on the thermal analysis techniques for assessing grain-refining characteristics during master alloy processing.