There are several main sources of thermophysical property data that provide the most authoritative and comprehensive compilations of critically and systematically evaluated data that are presently available. This article provides thermophysical property data to assist in the materials properties selection for the simulation of casting processes. The measurements of thermophysical property are difficult due to high temperatures and the reactivity of some alloys. The article discusses the strategies adopted to minimize the effects of high temperatures and reactivity of alloys. It presents the thermophysical properties of pure metals and some commercial alloys and tabulates the enthalpy of fusion and...