Lost Foam Casting
-
Published:2008
Abstract
This article discusses the sequence of operations for producing a foam pattern for casting. It provides information on expandable polystyrene, the most preferred material for manufacturing lost foam patterns. The article then describes the major functions of pattern molding and assembly. The types and application methods of various lost foam coatings are explained. The article also describes the investment of the foam pattern in a sand system. It concludes with a discussion on the advantages of lost foam casting and information on the formation and control of folds.
Sign in
ASM members
Member Sign InRaymond Donahue, Kevin Anderson, Lost Foam Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 640–645, https://doi.org/10.31399/asm.hb.v15.a0005254
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!