Processing and Finishing of Castings
-
Published:2008
Abstract
After solidification and cooling, further processing and finishing of the castings are required. This article describes the general operations of shakeout, grinding, cleaning, and inspection of castings, with particular emphasis on automation technology. It illustrates the vertical core knockout machine and the A-frame core knockout machine and lists the advantages and disadvantages of these machines. The article describes the general factors in automated or manual gate removal process. It concludes with discussion on the various types of inspection, such as the liquid penetrant inspection, pressure testing, radiographic inspection, magnetic particle inspection, and ultrasonic inspection.
Sign in
ASM members
Member Sign InProcessing and Finishing of Castings, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 513–521, https://doi.org/10.31399/asm.hb.v15.a0005355
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!