Titanium and Titanium Alloy Castings
-
Published:2008
Abstract
The combination of high strength-to-weight ratio, excellent mechanical properties, and corrosion resistance makes titanium the best material choice for many critical applications. This article begins with a description of the historical perspective of titanium casting technology. It discusses the types of molding methods, such as rammed graphite molding and lost-wax investment molding. The article provides information on the casting design, melting, postcasting, and pouring practices. It describes the microstructure and mechanical properties of Ti-6AI-4V alloy. The article examines the product applications of titanium alloy castings. The tensile properties, standard industry specifications, and chemical compositions of various titanium alloy castings are tabulated.
Mustafa Guclu, Titanium and Titanium Alloy Castings, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 1128–1142, https://doi.org/10.31399/asm.hb.v15.a0005337
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.