Numerical Methods for Casting Applications[1] Available to Purchase
-
Published:2008
Abstract
Computational fluid dynamics (CFD) is one of the tools available for understanding and predicting the performance of thermal-fluids systems. This article qualitatively describes the basic principles of CFD. The numerical methods, such as geometry description and discretization, used to solve the CFD equations are discussed. The article also demonstrates the application of CFD to a few casting problems.
Numerical Methods for Casting Applications, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 419–424, https://doi.org/10.31399/asm.hb.v15.a0005233